ALAŞIMSIZ GENEL YAPI ÇELİKLERİ |
Standard: EN 10025-Part 2-2004 |
Kimyasal Bileşim (%) |
Tosçelik Kalite No |
Standart |
Kalite |
|
C (maks.) |
Mn |
P |
S |
Cu |
Al(1) |
N(1) |
Ceq(2) |
d≤16 |
16 |
max |
max |
max |
max |
min |
max |
max |
TOS3750 |
EN 10025-2 |
S235JR |
Standart |
0.17 |
0.17 |
1.4 |
0.035 |
0.035 |
0.55 |
- |
0.012 |
0.35 |
TOS3751 |
EN 10025-2 |
S235JR+N |
Standart |
0.17 |
0.17 |
1.4 |
0.025 |
0.025 |
0.55 |
0.200 |
- |
0.35 |
TOS3752 |
EN 10025-2 |
S235J2+N |
Standart |
0.17 |
0.17 |
1.4 |
0.025 |
0.025 |
0.55 |
0.200 |
- |
- |
TOS4450 |
EN 10025-2 |
S275JR |
Standart |
0.21 |
0.21 |
1.4 |
0.035 |
0.035 |
0.55 |
- |
0.012 |
0.40 |
TOS4453 |
EN 10025-2 |
S275J2+N |
Standart |
0.18 |
0.18 |
1.4 |
0.035 |
0.035 |
0.55 |
0.200 |
- |
0.40 |
ALAŞIMSIZ GENEL YAPI ÇELİKLERİ |
Standard: EN 10025-Part 2-2004 |
Kimyasal Bileşim (%) |
Tosçelik Kalite No |
Standart |
Kalite |
|
C (maks.) |
Si |
Mn |
P |
S |
Cu |
Al(1) |
N(1) |
Ceq(2) |
d≤16 |
16 |
max |
maks |
max |
max |
max |
min |
max |
max |
TOS5221 |
EN 10025-2 |
S355J0 |
Standart |
0.20 |
0.20 |
0.55 |
1.6 |
0.030 |
0.030 |
0.55 |
- |
0.012 |
0.45 |
TOS5250 |
EN 10025-2 |
S355JR |
Standart |
0.24 |
0.24 |
0.55 |
1.6 |
0.035 |
0.035 |
0.55 |
- |
0.012 |
0.45 |
TOS5227 |
EN 10025-2 |
S355J2 |
Standart |
0.20 |
0.20 |
0.55 |
1.6 |
0.025 |
0.025 |
0.55 |
- |
- |
0.45 |
TOS5652 |
EN 10025-2 |
S355J2+N(1) |
Standart |
0.20 |
0.20 |
0.55 |
1.6 |
0.025 |
0.025 |
0.55 |
0.020 |
- |
0.45 |
Açıklamalar
1) Çeliğin kimyasal bileşiminde minimum %0.020 alüminyum olduğu takdirde azot üst sınırı uygulanmaz
2) Ceq hesabı için %CE (IIW) = C+Mn/6+(C+Mo+V)/5+(Ni+Cr)/15 formülü kullanılır.
ALAŞIMSIZ GENEL YAPI ÇELİKLERİ |
Standard: EN 10025-Part 2-2004 |
MEKANİK ÖZELLİKLER |
Tosçelik Kalite No |
Standart |
Kalite |
Re |
Rm(2) |
A(%), min. |
Darbe(boy)(3) |
N/mm² |
N/mm² |
A80 |
A5 |
|
KVc |
min. |
min. |
|
|
|
|
d : kalınlık, mm |
d : kalınlık, mm |
d : kalınlık, mm |
Sıc. |
min |
|
16 |
<3 |
3 ≤ d< 40 |
1 < d ≤ 1.5 |
1.5 < d ≤ 2 |
2 < d ≤ 2.5 |
2.5 < d ≤ 3 |
3 ≤ d ≤ 40 |
ºC |
J |
TOS5221 |
EN 10025-2 |
S355J0 |
355 |
345 |
510-680 |
470-630 |
13 |
14 |
15 |
16 |
20 |
0 |
27(4) |
TOS5250 |
EN 10025-2 |
S355JR |
355 |
345 |
510-680 |
470-630 |
13 |
14 |
15 |
16 |
20 |
20 |
27 |
TOS5227 |
EN 10025-2 |
S355J2 |
355 |
345 |
510-680 |
470-630 |
13 |
14 |
15 |
16 |
20 |
-20 |
27(4) |
TOS5652 |
EN 10025-2 |
S355J2+N(1) |
355 |
345 |
510-680 |
470-630 |
13 |
14 |
15 |
16 |
20 |
-20 |
27 |
Açıklamalar
1) Kalite kodunda “+N“ olan kaliteler için, müşteri tarafından “sıcak şekillendirme“ ve/veya “normalize“ işlemi yapılabilir.
2) Çekme testi değerleri “Enine“ test numunelerine uygulanır.
3) Kalınlığı 6 mm’nin altında olan ürünler için darbe testi uygulanmaz.
4) Darbe testi isteğe bağlı yapılır.